2024-12-18Glass Pre-Processing Requirements Before Entering a Glass Temperin…
To ensure optimal results, several important steps must be completed before glass is introduced into a glass tempering furnace.
-
2024-11-18What Causes Hot Spots on Tempered Glass?
Hot spots, also referred to as surface defects, are a common quality issue in tempered glass production. Hot spots on tempered glass generally fall into two categories: dispersed spots and dense spots.
-
2024-10-23How to Identify Tempered Glass Without Breaking It
There is a non-destructive method to identify tempered glass: A reliable way is to check for air marks, iridescence, or anisotropy—all of which indicate the presence of internal stress.
-
2024-09-25Tempering Low-Iron Glass: Essential Guidelines
When tempering low-iron glass, specific adjustments are necessary to accommodate its unique properties. First, it requires a longer heating time compared to normal float glass.
-
2024-08-14Is Laminated Annealed Glass Safety Glass?
Laminated glass is a type of safety glass composed of two or more layers of glass with one or more thin polymer interlayers between them.
-
2024-07-22How to Reduce Energy Consumption in Glass Tempering ?
Glass tempering furnaces are a major source of electricity consumption in factories. Reducing energy consumption in the glass tempering furnaces can lead to substantial cost savings.
-
2024-03-26Heating Time Standards for Glass Tempering Furnaces
Regarding the heating time of the glass tempering machine, we have strict standards.
-
2024-02-20How to Properly Shut Down a Glass Tempering Furnace?
Properly shutting down a glass tempering furnace involves a series of steps to ensure the furnace cools down safely and to prevent potential damage.